Texaco Molytex® EP NLGI Grade 0

 

Subcategory: Fluid; Lubricant

Close Analogs: CPS Number: 221920; MSDS Number: 8805

Material Notes:
Texaco Molytex EP grease delivers value through:

  • Good water resistance — Seals out water, reducing rust and corrosion.
  • Extreme pressure protection.
  • Protection against shock loading, extending vehicle life.
  • Good low temperature pumpability — Better low temperature performance means better handling in the container and grease-dispensing equipment.
  • Molybdenum disulfide for additional boundary lubrication protection.

Texaco Molytex EP greases are multipurpose, water resistant, extreme pressure general purpose lubricating greases.

They are manufactured using selected highly refined high viscosity index base oils, a lithium soap, a 3% molybdenum disulfide ("moly") antiwear agent, plus oxidation and rust inhibitors. It is dark gray in color and buttery in texture.

Texaco Molytex EP is available in two grades:

  • NLGI 0 for better pumpability at low ambient temperatures
  • NLGI 2 for normal ambient temperatures.

Texaco Molytex EP grease is designed especially for use in construction, mining and agricultural equipment.

Texaco Molytex EP grease strongly resists being washed out of bearings. It is stable and retains its consistency under adverse service conditions and protects parts over long service intervals.

Texaco Molytex EP grease has an outstanding film strength which results in particularly effective protection in shock load and extreme pressure service. The antiwear properties are enhanced by the molybdenum disulfide.

Texaco Molytex EP greases are recommended as multipurpose product for the lubrication of both over-the-road and off highway trucks, tractors, and heavy duty equipment.

They give excellent performance in all automotive equipment in severe service.

They provide top protection to fifth wheels, king pins, wheel bearings, steering system bearings, and all chassis points including ball joints and universal joints.

They also perform well in most heavy duty industrial applications for general lubrication and for the lubrication of journal bearings, and low and moderate speed antifriction bearings.

They are particularly effective in applications where high EP is desirable.

They perform well under high tempeature, wet, and dusty operating conditions.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

Available Properties
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Penetration P(0), 1/10 mm
  • Penetration P(60), 1/10 mm
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point
  • Flash Point
  • Dropping Point
  • Color
  • Molybdenum Disulfide, wt%
  • Texture
  • Thickener, %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。