Texaco Multifak® HD NLGI Grade 00

 

Subcategory: Fluid; Lubricant

Close Analogs: CPS Number: 221988; MSDS Number: 9006

Material Notes:
Texaco Multifak HD delivers value through:

  • Semi-fluid grease properties provide a thick film of lubricant to critical parts.
  • Low temperature lubrication.
  • Excellent rust and corrosion protection
  • Tacky consistency reduces the risk of water washout.

Texaco Multifak HD is a lithium based semi-fluid grease specially formulated with a high viscosity base oil, and an additive package that contains inhibitors and tackifiers.

Texaco Multifak HD is recommended for gear drives that specify an NLGI 00 grease. These include large mowing machines pulled behind tractors and gearboxes in large mixers.

Texaco Multifak HD is unsuitable for applications requiring an extreme pressure grease.

It is recommended for gear drives specifying a semifluid grease, including those manufactured by:

  • Jacobsen Division of Textron
  • NORD Gear Corporation

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.
  4. Unknown amount of work.

Available Properties
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Penetration
  • Penetration P(60), 1/10 mm
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Dropping Point
  • Color
  • Rust Prevention
  • Texture
  • Thickener, %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。