Texaco Thermatex® EP NLGI Grade 1

 

Subcategory: Fluid; Lubricant

Close Analogs: CPS Number: 222313; MSDS Number: 8707

Material Notes:
Texaco Thermatex EP greases deliver value through:

  • High temperature stability — Will not melt at high temperatures, but will remain in place on bearing surfaces and continue to provide excellent lubricity.
  • High film strength — High film strength assures good performance under heavy load and shock load conditions. Minimizes wear.
  • Leak prevention — Grease makeup prevents leakage and water washout from bearings.
  • High temperature performance — No-melt silica thickener keeps lubricant in place at high temperature conditions.

Texaco Thermatex EP are organoclay greases.

They are manufactured using high viscosity, high viscosity index base oils and contain effective rust and oxidation inhibitors.

Texaco Thermatex EP greases provide outstanding lubrication in industrial applications where extremely high temperatures are encountered. The dropping points of Texaco Thermatex EP exceed 260°C (500°F).

Texaco Thermatex EP greases have very high film strength and perform well under shock load conditions. They minimize wear and prevent scuffing.

Their high viscosity oil and high viscosity additive characteristics enable these lubricants to seal bearings and resist leakage and washout.

Under high temperature operating conditions, the "no melt" thickener keeps the lubricant in place long after conventional multipurpose greases would have melted and run out of bearings.

Texaco Thermatex EP greases have excellent pumpability characteristics.

Texaco Thermatex EP greases are recommended for industrial applications subjected to very high temperatures where a lubricant which will not melt is required.

Typical applications are plain or journal bearings, antifriction bearings, gear cases in kiln cars, conveyors in ceramic and paint baking ovens furnace doors, shafts extending through furnaces, etc.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

Available Properties
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Penetration P(60), 1/10 mm
  • Timken Test
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flash Point
  • Dropping Point
  • Color
  • Texture
  • Thickener, %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。