Texaco Transultex® CF G
Subcategory: Fluid
Close Analogs: CPS Number: 221553; MSDS Number: 8968
Material Notes: Texaco Transultex CF metalworking fluids deliver value through:- Excellent antiweld properties from active sulfur and chlorine-free EP compounding which reduce frictional heat, prevent welding of metal to the tool point, extend tool life and reduce power consumption in moderate to severe duty operations.
- Transparent, light color allows operator to better see the machined part during the cutting operation.
- Antimist control - Minimizes the amount of stray mist in the air around the machine and operator.
Texaco Transultex CF cutting oils are transparent, light color, low odor cutting oils containing active sulfur and chlorine-free EP compounding. These effective antiweld additives react at the chip-tool interface to form boundary lubricating films that reduce frictional heat and prevent welding of the tool and workpiece. Texaco Transultex CF cutting oils contain effective antiweld additives that react at the chip-tool interface to form boundary lubricating films that reduce frictional heat and prevent welding of the tool and workpiece. The chlorine-free nature of these cutting oils addresses many of the issues associated with chlorinated cutting oils, such as storage and waste disposal. Transultex CF cutting oils are preferred over chlorinated cutting oils for heavy duty machining of difficult nonferrous metals (e.g. titanium, nickel) that are not subject to staining, but may become brittle through the use of chlorinated fluids. Texaco Transultex CF cutting oils are formulated with paraffinic base stocks with naturally high viscosity index. These cutting oils have high flash points, minimizing the potential for fire. They also contain an effective mist control agent that reduces stray mist around the machine. This improves shop cleanliness and reduces operator exposure to the cutting oil. Texaco Transultex CF metalworking fluids: - Provide excellent cooling and lubrication in a wide range of machining operations
- Prevent welding of chip and tool
- Flush chips away from the work area
- Protect the finished work surfaces, tools and machines against rusting and staining
- Dramatically reduce oil mist in high speed machine tools
Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.
| Available Properties |
- API Gravity
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- ASTM Color
- Flash Point
- Calcium
- Chlorine
- Fatty Oil
- Phosphorus
- Sulfur
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|