Texaco Anti-Freeze/Coolant

 

Close Analogs: CPS Number: 222353; MSDS Number: 10298

Material Notes:

Texaco Anti-Freeze Coolant is a universal, low silicate, all purpose coolant designed for use in both automotive engines and heavy-duty diesel engines, particularly those containing aluminum alloys.

Texaco Anti-Freeze Coolant is a single phase, ethylene glycol based product blended with a premium quality additive package. It is a universal low silicate coolant designed for use in both heavy-duty diesel and automotive engines, particularly those containing aluminum alloys. This product provides antifoam properties, and rust and corrosion protection for aluminum, brass, copper, solder, steel and cast iron. It mixes readily with any clean tap water and is compatible with cooling system filters and supplemental additives.

Texaco Anti-Freeze Coolant is free of nitrites and amines.

In service Texaco Anti-Freeze Coolant provides:

  • Universal formula for both automotive and heavy-duty diesel engines (ASTM D 3306 and ASTM D 4985)
  • Aluminum corrosion protection
  • Heat transfer properties
  • Antifoam characteristics
  • Corrosion protection for aluminum, brass, copper, solder, steel and cast iron
  • Low silicate formulation
  • Nitrite-free, amine-free and borax free
  • Mixes readily with clean tap water
  • Compatible with cooling system filters
  • Compatible with heavy duty diesel supplemental coolant additives
  • Compatible with most major brands of coolant

Texaco Anti-Freeze Coolant is specially formulated to meet the stringent aluminum corrosion protection requirements of automotive engines. Because of its low concentration of silicate, it also complies with Cummins and other heavy-duty diesel engine manufacturers silicate requirements. This product is also suitable for use in industrial internal combustion engines where an antifreeze/coolant is required to provide protection against freezing, boil over, and corrosion. Texaco Anti-Freeze Coolant does not meet DEX COOL® requirements.

Note: These products are not to be used to protect the inside of potable water systems against freezing.

Texaco Anti-Freeze Coolant meets:

  • ASTM D 3306 for automotive service
  • ASTM D 4985 for heavy duty diesel service

Texaco Prediluted 50/50 Anti-Freeze Coolant meets:
  • ASTM D 4656 for pre-blend automotive service
  • ASTM D 5345 for pre-blend heavy duty diesel service

Texaco Anti-Freeze Coolant meets or exceeds the requirements of the following specifications: (It should be noted that many heavy-duty diesel manufacturers are changing their requirements to simply require ASTM D 4985.): AAMVA; General Motors - GM1825M, GM 1899M (performance corresponding to GM 6038M); ASTM D 3306 including ASTM D 4340, ASTM D 4985; Chrysler MS-7170; Cummins 90T8-4; Detroit Diesel Corp; Federal Specification A-A-870; Ford ESE-M97B44-A; Freightliner; J.I. Case JIC 501; John Deere H24B1, H24C1; Mack Truck; PACCAR; SAE J1034; TMC of ATA RP-302A.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Negative indicates net gain.

Available Properties
  • Specific Gravity
  • pH
  • Melting Point
  • Appearance
  • Glassware Corrosion Test, Aluminum
  • Glassware Corrosion Test, Brass
  • Glassware Corrosion Test, Copper
  • Glassware Corrosion Test, Iron
  • Glassware Corrosion Test, Solder
  • Glassware Corrosion Test, Steel
  • Reseve Alkalinity (mL)
  • Silicate %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。