DSM Somos 9920
Subcategory: Polymer; Stereolithography (SLA®); Clear; Amber; Paintable; General Purpose; Snap-fit / Functional Testing; Cast Urethane Pattern; Concept Models; Show Model; Medical Grade; Fine Detail (High Resolution); Can be Plated (Nickel, Copper); Smooth Surface
Material Notes: View the manufacturer data sheet.
| Available Properties |
- Viscosity
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|