Platinum, Pt, CP Grade, Annealed
Subcategory: Metal; Nonferrous Metal; Precious Metal; Pure Element
Component | Wt. % | | | Pt | 99.95 | |
|
Material Notes: CP Grade (Commercially Pure) is 99.95% pure.
Click here to view available vendors for this material.
Physical Properties | Metric | English | Comments |
|
Density | 21.45 g/cc | 0.775 lb/in³ | |
Mechanical Properties |
|
Hardness, Vickers | 40 | 40 | |
Tensile Strength, Ultimate | 125 - 165 MPa | 18100 - 23900 psi | |
Elongation at Break | 35 % | 35 % | in 50 mm |
Modulus of Elasticity | 171 GPa | 24800 ksi | static in tension |
Poisson's Ratio | 0.39 | 0.39 | |
Shear Modulus | 62 GPa | 8990 ksi | Calculated value |
Electrical Properties |
|
Electrical Resistivity | 1.06e-005 ohm-cm | 1.06e-005 ohm-cm | Temperature Coefficient of resistivity is 0.0039/K. |
Magnetic Susceptibility | 1.1e-006 | 1.1e-006 | cgs/g |
Thermal Properties |
|
Heat of Fusion | 113 J/g | 48.6 BTU/lb | |
CTE, linear 20°C | 9.1 µm/m-°C | 5.06 µin/in-°F | |
Specific Heat Capacity | 0.134 J/g-°C | 0.032 BTU/lb-°F | |
Thermal Conductivity | 69.1 W/m-K | 480 BTU-in/hr-ft²-°F | |
Melting Point | 1769 °C | 3220 °F | |
Optical Properties |
|
Emissivity (0-1) | 0.152 | 0.152 | at 1000°C for total hemispherical |
Emissivity (0-1) | 0.3 | 0.3 | 650 nm |
Reflection Coefficient, Visible (0-1) | 0.7 | 0.7 | bulk Pt; 589 nm |
|
Printer friendly version |
References for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
|