AISI Type 420 Stainless Steel, tested at 205°C (400°F)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Ferrous Metal; Heat Resisting; Metal; Stainless Steel; T 400 Series Stainless Steel

Key Words: UNS S42000, AMS 5506, AMS 5621, ASTM A276, ASTM A314, ASTM A473, ASTM A580, FED QQ-S-763, FED QQ-S-766, FED QQ-W-423, MIL SPEC MIL-S-862, SAE J405 (51420), B.S. 420 S 37, B.S. CDS-18 (U.K), martensitic, DIN 1.4021, AFNOR Z 20 C 13 (Fr), UNI X 20 Cr 13, JIS SUS 420 J1, SS14 2303 (Sweden), ISO 683/13 4

Component   Wt. %
CMin 0.15 
Cr13 
Fe85 
MnMax 1 
PMax 0.04 
SMax 0.03 
SiMax 1 

Material Notes:
16.0 mm diameter bar, austenitized at 980°C for 30 minutes, oil quench, temper for 2 hours at 28°C above test temperature

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesMetricEnglishComments
Density7.8 g/cc0.282 lb/in³ 

Mechanical Properties
Hardness, Brinell506506 Converted from Rockwell C Hardness
Hardness, Knoop562562 Converted from Rockwell C Hardness
Hardness, Rockwell C51.551.5 before testing, 51 after
Hardness, Vickers541541 Converted from Rockwell C Hardness
Tensile Strength, Ultimate1820 MPa264000 psi 
Tensile Strength, Yield1085 MPa157000 psi at 0.2% offset
Elongation at Break11.5 %11.5 % in 50 mm
Charpy Impact100 J73.8 ft-lb annealed (tested at room temperature), 14 J quenched and tempered (tested at room temperature)
Shear Modulus80.7 GPa11700 ksi 

Electrical Properties
Electrical Resistivity5.5e-005 ohm-cm5.5e-005 ohm-cm at 20°C

Thermal Properties
CTE, linear 20°C10.3 µm/m-°C5.72 µin/in-°F from 0-100°C (32-212°F)
CTE, linear 250°C10.8 µm/m-°C6 µin/in-°F at 0-315°C (32-600°F)
CTE, linear 500°C11.7 µm/m-°C6.5 µin/in-°F 0-540°C, 12.2 at 0-650°C
Specific Heat Capacity0.46 J/g-°C0.11 BTU/lb-°F from 0-100°C (32-212°F)
Thermal Conductivity24.9 W/m-K173 BTU-in/hr-ft²-°F at 100°C
Melting Point1455 - 1510 °C2650 - 2750 °F 
Solidus1455 °C2650 °F 
Liquidus1510 °C2750 °F 
Maximum Service Temperature, Air620 °C1150 °F Continuous Service
Maximum Service Temperature, Air735 °C1360 °F Intermittent Service
Printer friendly version Printer friendly version

References for this datasheet.


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ASM International

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。