RTP Company RTP 1405 HF TFE 15 Polyethersulfone (PES) Glass Fiber 30% - PTFE 15% - High Flow

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)Material suppliers Material suppliers
 Export data to your CAD/FEA program

Subcategory: Polyethersulfone; Polymer; Thermoplastic

Close Analogs:
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Material Notes:
Glass Fiber 30% - PTFE 15% - High Flow

Comments:

  • Glass Fiber
  • PTFE Lubricated
  • High Flow

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.

Click here to view available vendors for this material.

Physical PropertiesMetricEnglishComments
Specific Gravity1.69 g/cc0.0611 lb/in³ ASTM D792
Filler Content30 %30 % 
Linear Mold Shrinkage0.005 cm/cm0.005 in/in 1/8 inch (3.18 mm) section; ASTM D955

Mechanical Properties
Tensile Strength, Ultimate110 MPa16000 psi ASTM D638
Elongation at Break1.4 %1.4 % ASTM D638
Modulus of Elasticity10.3 GPa1500 ksi ASTM D638
Flexural Modulus8.96 GPa1300 ksi ASTM D790
Flexural Yield Strength172 MPa25000 psi ASTM D790
Izod Impact, Unnotched4.81 J/cm9 ft-lb/in 1/8 in (3.18 mm) section; ASTM D256
Izod Impact, Notched1.07 J/cm2 ft-lb/in 1/8 in (3.18 mm) section; ASTM D256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)204 °C400 °F ASTM D648

Processing Properties
Processing Temperature343 - 366 °C650 - 690 °F 
Mold Temperature135 - 177 °C275 - 350 °F 
Injection Pressure68.9 - 103 MPa10000 - 15000 psi 

Descriptive Properties
ColorNatural/Black 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Specialty Compounds RTP Company

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。