RTP Company ESD C 1480 N Polyethersulfone (PES) Conductive - Carbon Fiber - High Viscosity
Subcategory: Polyethersulfone; Polymer; Thermoplastic 
Close Analogs:  Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade. 
Material Notes:  Conductive - Carbon Fiber - High Viscosity Comments: - Conductive
 - ESD Protection
 - Carbon Fiber
 - High Viscosity
 
 Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company. 
Click here to view available vendors for this material. 
| Physical Properties | Metric | English | Comments |  
 |  
| Specific Gravity | 1.39 g/cc | 0.0502 lb/in³ |  ASTM D792 |  
| Water Absorption | 0.4 % | 0.4 % |  24 hours at 23°C; ASTM D570 |  
| Linear Mold Shrinkage | 0.002 cm/cm | 0.002 in/in |  1/8 inch (3.18 mm) section; ASTM D955 |  
| Linear Mold Shrinkage, 6.35 mm section | 0.004 cm/cm | 0.004 in/in |  1/4 inch (6.35 mm) section; ASTM D955 |  
 Mechanical Properties |  
 |  
| Tensile Strength, Ultimate | 103 MPa | 15000 psi |  ASTM D638 |  
| Elongation at Break | 3 - 4 % | 3 - 4 % |  ASTM D638 |  
| Modulus of Elasticity | 5.86 GPa | 850 ksi |  ASTM D638 |  
| Flexural Modulus | 5.17 GPa | 750 ksi |  ASTM D790 |  
| Flexural Yield Strength | 165 MPa | 24000 psi |  ASTM D790 |  
| Izod Impact, Unnotched | 5.34 J/cm | 10 ft-lb/in |  1/8 in (3.18 mm) section; ASTM D256 |  
| Izod Impact, Notched | 0.534 J/cm | 1 ft-lb/in |  1/8 in (3.18 mm) section; ASTM D256 |  
 Electrical Properties |  
 |  
| Electrical Resistivity | 1000 - 1e+009 ohm-cm | 1000 - 1e+009 ohm-cm |  ASTM D257 |  
| Surface Resistance | 1e+006 - 1e+012 ohm | 1e+006 - 1e+012 ohm |  ASTM D257 |  
| Static Decay | Max 2 sec | Max 2 sec |  FTMS-4046.1 |  
 Thermal Properties |  
 |  
| Deflection Temperature at 0.46 MPa (66 psi) | 207 °C | 405 °F |  ASTM D648 |  
| Deflection Temperature at 1.8 MPa (264 psi) | 204 °C | 400 °F |  ASTM D648 |  
| Flammability, UL94 | V-0 | V-0 |  (V-0) at 0.06 in (1.5 mm); Per testing by RTP Company; ASTM D3801 |  
 Processing Properties |  
 |  
| Processing Temperature | 343 - 366 °C | 650 - 690 °F |   |  
| Mold Temperature | 135 - 177 °C | 275 - 350 °F |   |  
| Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi |   |  
 Descriptive Properties |   |  
| Color | Natural/Black |   |  
 |  
  Printer friendly version |  
 
   Some of the values displayed above may have been converted from their original units and/or rounded in
  order to display the information in a consistant format.  Users requiring more precise data for scientific or
  engineering calculations can click on the property value to see the original value as well as raw conversions
  to equivalent units.  We advise that you only use the original value or one of its raw conversions in your
  calculations to minimize rounding error.  We also ask that you refer to MatWeb's disclaimer and terms of use